Nanovea is proud to announce the arrival of the new redesigned Tribometer!

Nanovea Tribometer

NEWS__________________________________________________________________________

FOR IMMEDIATE RELEASE

Nanovea Launches Redesigned Tribometer With 3D Optical Profiler Integration


Pin-On-Disk TribometerThe release of the New Nanovea Tribometer marks the end to bulky, unappealing and complicated Tribology testing. Nanovea’s Tribometer has been redesigned to complete Nanovea’s signature instrument look and user-friendly appeal. The Nanovea Tribometer also introduces, to the world of Tribology, quick in-situ 3D Optical Profiler integration for wear calculation analysis along with other 3D surface measurements. In addition, the Nanovea Tribometer can reach speeds of 6000rpm. To offer the same quality data at these high speeds, Nanovea has integrated a fast 56000Hz acquisition card with 24bit resolution. The system also comes standard with a motorized table that allows to precisely position the arm through computer control.

The diverse capabilities of Nanovea’s Tribometer design allows for Pin-On-Disk and Linear Reciprocating modules. Testing abilities include high temperature testing up to 1000C, Tri-mode lubrication system and several other enhanced environment testing options. A precision RVDT can be used to measure the change of vertical displacement during testing. The value given may be used to manually calculate the sample’s wear rate.  The optional 3D Optical Profiler provides the user a software automated option for calculating wear rate. This optional feature will also be useful for quick and easy analysis of roughness, critical dimensions, topography and full pre and post test area profile. Nanovea Tribometer Software gives users the ability to easily control test parameters including: speed, frequency, contact pressure and varying time. To mimic a specific range of applications Nanovea’s Tribometer can be built with custom adjustments.

The Tribology industry needs a star instrument, one with the refined design and advanced user friendly technology. I think Nanovea has delivered.—Susana Cabello Product Manager

LABORATORY___________________________________________________________________

Laboratory Services Examples of what we tested this month:

Mechanical:
Nanoindentation & adhesion of DLC coating on foil substrate
Nanoindentation & adhesion of blu-ray discs
Nanoscale Scratch marking on microchips
3D Non-Contact Metrology:
Wear loss on metal
Photovoltaic Wafer roughness, flatness & thickness
Solar thin film step height
Microchip replica verification and analysis
Microwire roughness
Fresnel lens topography
Blister Pack thickness & analysis
Fuel cell roughness, flatness & thickness
Tribology:
Coefficient of friction comparison of lubrication solutions
Coefficient of friction of wafer and steel coupon


APPLICATION NOTES____________________________________________________________

THIS MONTH:

Coefficient of Friction of Eye Drop Solution


              Eye Drop Solution                     Coefficient of Friction Testing


Nanoindentation of Silicon Carbide Wafer


               Silicon Carbide Wafer                  
Nanoindentation on Silicon Carbide              

      
Silicon Wafer Flatness With 3D Metrology

              Silicon Wafer                       3D Wafer Flatness         

                     
PREVIOUS MONTHS:

Solar Cell Surface Inspection With 3D Metrology

Battery Contact Wear Loss With 3D Metrology

Hardness of Bulk Materials With Instrumented Indentation

Aspheric Lens Topography With 3D Non-Contact Metrology

Wear Resistance Analysis With Tribometer Friction Measurements

Quality Control Comparison of Tablet Roughness

Wear Rate Analysis Using Tribology & 3D Metrology


TRADESHOWS__________________________________________________________________

COMING MONTHS:

MS&T Pittsburgh, PA - October 25-29